KRISHI
ICAR RESEARCH DATA REPOSITORY FOR KNOWLEDGE MANAGEMENT
(An Institutional Publication and Data Inventory Repository)
"Not Available": Please do not remove the default option "Not Available" for the fields where metadata information is not available
"1001-01-01": Date not available or not applicable for filling metadata infromation
"1001-01-01": Date not available or not applicable for filling metadata infromation
Please use this identifier to cite or link to this item:
http://krishi.icar.gov.in/jspui/handle/123456789/47131
Full metadata record
DC Field | Value | Language |
---|---|---|
dc.contributor.author | S. N. Chattopadhyay, N. C. Pan, A. N. Roy and Kartick K. Samanta, and A. Khan | en_US |
dc.date.accessioned | 2021-06-06T12:08:04Z | - |
dc.date.available | 2021-06-06T12:08:04Z | - |
dc.date.issued | 2020-09-01 | - |
dc.identifier.citation | Not Available | en_US |
dc.identifier.issn | Not Available | - |
dc.identifier.uri | http://krishi.icar.gov.in/jspui/handle/123456789/47131 | - |
dc.description | Not Available | en_US |
dc.description.abstract | Bleaching of jute has become essential for making white glossy fabric or base material for coloration intended for value added and diversified products. The conventional hot hydrogen peroxide bleaching process produces white fiber with high loss of tensile strength and impairing the feel. On the other hand newly developed peracetic acid bleaching of jute produces minimum loss of tenacity without impairing the feel but whiteness achieved is slightly low. Partial bleaching of jute was carried out using 25%, 50%, and 75% of the normal dose of bleaching agents and their whiteness index as well as tensile strength were evaluated. In all the cases hydrogen peroxide produced 5–8 grade higher whiteness in HUNTER scale while peracetic acid bleached sample retains higher tensile strength. So, two-step bleaching was carried out using hydrogen peroxide and peracetic acid following single-bath and double-bath processes. Twostep single-bath bleaching of jute fabric using 75% peracetic acid followed by 25% hydrogen peroxide bleaching treatment results in best effect with respect to optical and physical properties. | en_US |
dc.description.sponsorship | Not Available | en_US |
dc.language.iso | English | en_US |
dc.publisher | Taylor & Francis | en_US |
dc.relation.ispartofseries | Not Available; | - |
dc.subject | Bleaching; jute fiber; hydrogen peroxide; peracetic acid; whiteness index; tensile properties | en_US |
dc.title | Two-Step Bleaching of Jute Yarn and Fabric Using Hydrogen Peroxide and Peracetic Acid | en_US |
dc.title.alternative | Not Available | en_US |
dc.type | Research Paper | en_US |
dc.publication.projectcode | Not Available | en_US |
dc.publication.journalname | Journal of Natural Fibres | en_US |
dc.publication.volumeno | Not Available | en_US |
dc.publication.pagenumber | Not Available | en_US |
dc.publication.divisionUnit | Not Available | en_US |
dc.publication.sourceUrl | https://doi.org/10.1080/15440478.2020.1821278 | en_US |
dc.publication.authorAffiliation | ICAR::National Institute of Research on Jute and Allied Fibre Technology | en_US |
dc.ICARdataUseLicence | http://krishi.icar.gov.in/PDF/ICAR_Data_Use_Licence.pdf | en_US |
dc.publication.naasrating | 8.62 | - |
Appears in Collections: | AEng-NINFET-Publication |
Files in This Item:
There are no files associated with this item.
Items in KRISHI are protected by copyright, with all rights reserved, unless otherwise indicated.