Weak charge-ordering behavior in phase separated (Ln(1/3)Sm(2/3))(2/3)Ca1/3MnO3 (Ln = Pr and La) manganites
DSpace at IIT Bombay
View Archive InfoField | Value | |
Title |
Weak charge-ordering behavior in phase separated (Ln(1/3)Sm(2/3))(2/3)Ca1/3MnO3 (Ln = Pr and La) manganites
|
|
Creator |
ASTHANA, S
DHO, J BAHADUR, D |
|
Subject |
colossal magnetoresistance
pr0.67ca0.33mno3 pr1-xcaxmno3 perovskite transition state manganites magnetoresistance colossal magnetoresistance electronic phase separation |
|
Description |
We have studied a weak charge-ordering behavior in phase separated (Ln(1/3)Sm(2/3))(2/3)Ca1/3MnO3 (Ln = Pr and La) manganites with same hole doping but slightly different tolerance factors. The M(T) and p(T) curves of the Pr-sample showed an anomaly caused by a weak charge-order (CO) transition at similar to 210 K. while that of La-sample did not. However, the La-sample displayed a weak anomaly related to the CO instability in the derivative curve of the temperature dependent magnetoresistance. This result is understood on the basis that the CO phase in La-sample is partly suppressed by a large magnetic field of similar to 80 kOe, while in Pr-sample it is not collapsed in that field scale. Our data support the existence of charge-ordering, electronic phase separation and a field-induced reduction of weak CO instability for La-sample, which can contribute towards high MR especially at lower temperatures due to partial melting of CO phase and/or percolation behavior. (c) 2007
|
|
Publisher |
PERGAMON-ELSEVIER SCIENCE LTD
|
|
Date |
2011-08-27T03:37:25Z
2011-12-26T12:57:43Z 2011-12-27T05:44:54Z 2011-08-27T03:37:25Z 2011-12-26T12:57:43Z 2011-12-27T05:44:54Z 2007 |
|
Type |
Article
|
|
Identifier |
SOLID STATE COMMUNICATIONS, 143 (11-12), 522-526
0038-1098 http://dx.doi.org/10.1016/j.ssc.2007.07.008 http://dspace.library.iitb.ac.in/xmlui/handle/10054/11530 http://hdl.handle.net/10054/11530 |
|