Effect of strain rate on twinning in a Zr alloy
DSpace at IIT Bombay
View Archive InfoField | Value | |
Title |
Effect of strain rate on twinning in a Zr alloy
|
|
Creator |
KAPOOR, R
SARKAR, A SINGH, J SAMAJDAR, I RAABE, D |
|
Subject |
Zr alloy
Tensile twin High strain rate Strain hardening COMMERCIALLY PURE TITANIUM ROOM-TEMPERATURE MECHANICAL-PROPERTIES DEFORMATION-BEHAVIOR PLASTIC-DEFORMATION CONSTITUTIVE LAW ZIRCONIUM TEXTURE MICROSTRUCTURE DISLOCATIONS |
|
Description |
Zr-1Nb alloy uniaxially compressed at room temperature at 10(-2) and 10(3) s(-1) exhibited twinning and a three-stage strain-hardening behavior. At 10(3) s(-1) the twin fraction initially increased to 0.3, decreasing to 0.02 at higher strains. Despite the difference in texture at intermediate strains, the final texture was similar at both strain rates. The increasing strain-hardening rate in the second stage was attributed to strengthening from grain boundaries and dislocations, and softening from reorientation due to twinning. (C) 2013 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
|
|
Publisher |
PERGAMON-ELSEVIER SCIENCE LTD
|
|
Date |
2014-12-29T05:13:37Z
2014-12-29T05:13:37Z 2014 |
|
Type |
Article
|
|
Identifier |
SCRIPTA MATERIALIA, 7472-75
1359-6462 http://dx.doi.org/10.1016/j.scriptamat.2013.10.025 http://dspace.library.iitb.ac.in/jspui/handle/100/17165 |
|