Finishing of jute using methacrylic acid in presence of tetrasodium pyrophosphate and potassium persulphate as catalysts under thermal treatment
NOPR - NISCAIR Online Periodicals Repository
View Archive InfoField | Value | |
Title |
Finishing of jute using methacrylic acid in presence of tetrasodium pyrophosphate and potassium persulphate as catalysts under thermal treatment
|
|
Creator |
Das, Debasish
Munshi, Rajiv |
|
Subject |
Cellulose
Esterification Finishing Graft copolymerization Jute Methacrylic acid |
|
Description |
82-90
Jute fabric has been modified using methacrylic acid as the finishing agent in the presence of K₂S₂O₈ and Na₄P₂O₇ catalysts separately or in selected combinations, employing a pad-batch-dry-cure technique. It is found that the treatment with 100g/L methacrylic acid at 30°C and pH 7 using batching time of 60-75 min at 30°C followed by drying of the batched fabric at 95°C for 5 min and curing of the dried fabric at 140°C for 5 min under the catalytic influence of K₂S₂O₈ and Na₄P₂O₇ produces most balanced improvement in the textile-related properties, such as wrinkle recovery angle, flexibility, abrasion resistance, elongation-at-break and resistance to photo-yellowing with retention of strength. |
|
Date |
2009-03-19T08:07:15Z
2009-03-19T08:07:15Z 2009-03 |
|
Type |
Article
|
|
Identifier |
0971-0426
http://hdl.handle.net/123456789/3388 |
|
Language |
en_US
|
|
Publisher |
CSIR
|
|
Source |
IJFTR Vol.34(1) [March 2009]
|
|