Ferro-Manganese Oxide Growth on Shark Teeth from Central Indian Ocean Basin
NOPR - NISCAIR Online Periodicals Repository
View Archive InfoField | Value | |
Title |
Ferro-Manganese Oxide Growth on Shark Teeth from Central Indian Ocean Basin
|
|
Creator |
Banakar, V K
Sudhakar, M |
|
Description |
265-269
Study of ferro-manganese oxide growth on apatitic substrates like shark teeth enamel from siliceous sediment environment (lat. 10 degrees S and long. 75 degrees E) suggests the changes in depositional environments within the sediment layer through the growth history of these oxides. Though the nature of substrates does not have any control over the mineralogy and chemistry of Fe-Mn oxides, an active sink like loose sediment or altered basaltic coat appears to be the primary requirement before ferric hydroxide coat on hard nucleating agent. |
|
Date |
2016-12-13T12:05:30Z
2016-12-13T12:05:30Z 1988-12 |
|
Type |
Article
|
|
Identifier |
0975-1033 (Online); 0379-5136 (Print)
http://nopr.niscair.res.in/handle/123456789/38570 |
|
Language |
en_US
|
|
Rights |
CC Attribution-Noncommercial-No Derivative Works 2.5 India
|
|
Publisher |
NISCAIR-CSIR, India
|
|
Source |
IJMS Vol.17(4) [December 1988]
|
|