Microstructure and Mechanical Properties of Magnesium-Aluminium (Mg-Al) Alloys with High Aluminium Content (Al =10, 15, 20 wt. %)
NOPR - NISCAIR Online Periodicals Repository
View Archive InfoField | Value | |
Title |
Microstructure and Mechanical Properties of Magnesium-Aluminium (Mg-Al) Alloys with High Aluminium Content (Al =10, 15, 20 wt. %)
|
|
Creator |
Jayalakshmi, S
Singh, R Arvind Mohan, Sanjay Sankaranarayanan, S Gomano, Vasco Machemba Chen, Xizhang Gupta, Manoj |
|
Subject |
Magnesium alloys
Aluminium Microstructure Intermetallic phase Mechanical behaviour |
|
Description |
184-189
Magnesium-Aluminium (Mg-Al) alloys containing zinc or manganese are preferred choice in automobile and aerospace sectors. Aluminium, the major strengthening element in Mg-alloys is always added below its solid solubility limit of 12.5 wt.%. In the current study, Mg-Al binary systems with Al-content just below and above the solubility limit (Al = 10, 15 and 20 wt.%,) were developed and examined for their microstructural and mechanical behaviour. Microstructural studies showed the importance of Al-content in determining: (i) grain size reduction and (ii) distribution and amount of inter metallic phase. Mechanical property evaluation showed that the hardness increase was linearly dependent on Al-content, with Mg-20Al showing > 250% increase in hardness than commercial AZ91alloy. Mg-10Al showed 215% and 130% increase in yield and ultimate strengths respectively, and exhibited the best properties in terms of work of fracture, which is representative of the alloy’s toughness. |
|
Date |
2021-03-16T07:11:33Z
2021-03-16T07:11:33Z 2021-03 |
|
Type |
Article
|
|
Identifier |
0975-0959 (Online); 0301-1208 (Print)
http://nopr.niscair.res.in/handle/123456789/56516 |
|
Language |
en_US
|
|
Rights |
CC Attribution-Noncommercial-No Derivative Works 2.5 India
|
|
Publisher |
NISCAIR-CSIR, India
|
|
Source |
IJPAP Vol.59(03) [March 2021]
|
|